36 cm Ytong exterior wall, solid construction, mold formation, insulation

  • Erstellt am 2012-09-13 08:29:06

kamnik

2012-10-28 14:18:08
  • #1


Problematic with Ytong in outdoor areas: If the outer skin is damaged and water penetrates,
the whole block swells like a sponge.
Just take a look at the pallets that have been standing in a puddle for a while?

Furthermore, I would never connect a PPW 6 with a calcium silicate block (see door and window frames). How else do you want to drill and anchor in such a soft material?

It seems to me the planners are moving further and further away from the basics. My tip: put on your rubber boots again and talk to the people on site. No idea how a full-time planner has so much time in life? It's like the angle lawyers who also fumble around in politics on the side? Better: focus on the day-to-day business?
 

€uro

2012-10-28 17:13:16
  • #2
Correct, one possibility among many!

Best regards.
 
Oben