Bob79
2019-07-07 18:55:40
- #1
Hello everyone,
on Friday our concrete slab was poured. For curing, it was first poured and then covered with foil. Due to the strong wind on Saturday, the foil has now blown away and the view of the concrete slab is now clear. I cannot see any cracks. But this morning it rained heavily and now you can see, due to the puddle formation, what I consider to be a quite significant unevenness (water stands on one side of the slab, the other side is already dry; with the same sunlight). I am also attaching a few pictures of the concrete slab. What do you think about it? Is the unevenness a defect? (Picture 1 Sunday afternoon several hours after the rain; Picture 2: Sunday morning directly after the rain; Picture 3: Saturday evening; Picture 4: reinforcement
)
on Friday our concrete slab was poured. For curing, it was first poured and then covered with foil. Due to the strong wind on Saturday, the foil has now blown away and the view of the concrete slab is now clear. I cannot see any cracks. But this morning it rained heavily and now you can see, due to the puddle formation, what I consider to be a quite significant unevenness (water stands on one side of the slab, the other side is already dry; with the same sunlight). I am also attaching a few pictures of the concrete slab. What do you think about it? Is the unevenness a defect? (Picture 1 Sunday afternoon several hours after the rain; Picture 2: Sunday morning directly after the rain; Picture 3: Saturday evening; Picture 4: reinforcement